Use LCP when the wall between pins is under about 0.3 mm, when the pitch is 1.27 mm or finer, or when coplanarity on a long body has to hold through reflow. On 2.54 mm parts with thick walls, PA6T or PA9T performs the same and costs less.

The reason is flow. LCP has very low melt viscosity and a highly ordered structure, so it fills thin sections and holds dimensions as it solidifies. That is exactly what a fine pitch housing needs and exactly what you pay for.

What LCP brings

Property LCP PA6T PBT
HDT 280–340 °C ~290 °C 200–210 °C
Minimum practical wall 0.15–0.2 mm 0.4–0.5 mm 0.6 mm
Warpage on long bodies Very low Low Moderate
Moisture absorption <0.04% ~2% ~0.1%
Relative cost High Medium Low

Why thin walls need it

At 1.27 mm pitch there is roughly 0.7 mm between adjacent pin holes, and the wall around each hole is a fraction of that. A polyamide at that thickness either short-shots in the mold or warps when it cools, because the flow front freezes before the cavity fills.

LCP fills it because the melt is nearly water-thin at processing temperature. The same property means the mold has to be well vented and the gate well designed, or the part flashes.

Warpage and coplanarity

Coplanarity on a long SMT header is a warpage problem. LCP’s low shrinkage and high stiffness keep a 40 mm body flat through reflow. That is why fine pitch board-to-board connectors are almost always LCP, and why 2.54 mm headers usually are not.

Where LCP is over-specified

  • 2.54 mm headers with 0.8 mm walls: PA6T holds coplanarity fine at this wall thickness.
  • Through-hole parts that never see reflow: PBT is adequate and much cheaper.
  • Parts with a metal shell carrying the structural load: the plastic is not doing the work.

The processing consequences

LCP is brittle at the pin exit. A pin inserted with too much interference will crack the wall, and the crack propagates. The pin hole tolerance has to be tighter than for PA6T, and the press force has to be controlled.

It also has a sharp melting point, which means the barrel temperature window in molding is narrow. That is a supplier capability question, not something a buyer can specify around.

Can LCP be used for wave solder parts?

Yes, but it is wasted. If the part never sees reflow, a cheaper material does the job.

Does LCP change the current rating?

No. The pin and plating set the rating. LCP only allows a denser pin field for the same rating.

Is LCP available in V-0?

Yes, most grades are UL94V-0. Ask for the yellow card and the thickness it applies to, because thin walls and thick walls often have different ratings.

Tell us the pitch and the wall thickness and we will say whether LCP is required or just comfortable. Fine pitch parts are quoted under board-to-board; the wider material comparison is in PA6T, PA9T or PBT.